Analysis of the causes of cold spot in the gate area of ​​injection molding products and solutions The cold spot mainly refers to the foggy or bright colored markings at the near gate of the workpiece or the curved scars on the top from the gate. They are caused by the plastic front entering the cavity or by the cold material that is squeezed into the cavity due to excessive pressure holding. The front material transfers heat due to the cooling action of the nozzle or the flow path, and is cooled and solidified before entering the cavity. When the injection cavity is expanded through the narrow gate, a melt fracture is formed, which is then pushed by the later hot melt, and thus becomes a cold spot.
Solution:
(1) The cold well should be opened. Also consider the form, size and location of the gate to prevent the material from cooling at a significant rate.
(2) The centering degree of the nozzle should be adjusted, and the matching size between the nozzle and the mold feeding should be designed to prevent leakage or cause cold material to be brought into the cavity.
(3) The mold discharge degree is good. Gas interference can cause turbid markings in the gate.
(4) Increase the mold temperature. Slow down the injection speed, increase the injection pressure, reduce the pressure holding and injection time, and reduce the holding pressure.
(5) Dry the plastic. Use less lubricant to prevent contamination of the powder.
Http://news.chinawj.com.cn Editor: (Hardware Business Network Information Center) http://news.chinawj.com.cn
Modern Soap Dispenser,Soap Dispenser For Vila,Soap Dispenser Pump For Sink,Kitchen Sink Soap Dispenser
Kaiping Jenor Sanitary Ware Co., Ltd , https://www.sanitaryjenor.com